Shit posting but 3d this time
Shit posting but 3d this time
Print failed because the layer adhesion is shit on my printer.
Shit posting but 3d this time
Print failed because the layer adhesion is shit on my printer.
If printing PLA, put a brine (salt solution) on your bed. PLA bonds with salt when warmed up (heated bed) and loses its bond when cooled off.
Is this legit? Or are you making a spaghetti joke? I actually can't tell lol
Here's a scientific paper about it. :) https://medialibrary.uantwerpen.be/oldcontent/container11343/files/bonding_pla_with_salt_water_v20160713.pdf
A brine is a much cleaner solution than the usual advices of hairspray or tape. Just be careful not to put salt on your electronics.