Hey everyone.

I built an mk3s+ from its kit form successfully, tested a few PLA prints with the stock 0.4 nozzle.

I've set prusaslicer to use a 0.6 nozzle now that I've upgraded, and am using PETG. Prints look pretty bad, in spite of calibrating z-offset etc.

If you were doing something like this for the first time, what would your setup steps be like?

To be specific, using a diamondback 0.6 nozzle, matterhackers PETG at 235c.

Issues I'm seeing are a really bad loss of detail, lots of stringing, etc.

eta: added a photo of a moderately post-processed part. Notice how rough the top surface looks, there's a disconnect between perimeter loops, etc.

19

You're viewing a single thread.

19 comments
  • I got PETG working on my Mini clone by basically just switching to 0.6 nozzle profiles from the wizard and using the generic PETG profile.

    But, if you’re new to PETG, know that it gets real moisture sensitive, real fast. Sounds like you might benefit from trying to dry the filament out, check the web for more on that.

    After making sure the filament was dry and that my initial layer is good, because changing nozzles means you need to fine tune the z offset again, I would print a retraction tower test and dial in retraction length settings.

    That a good basic troubleshooting list.